Written on: September 1, 2025 by W. Stephen Tait
Hello, everyone. I’ve often been asked how corrosion causes spray package failures. We’ll start by defining what is meant by a spray package failure by understanding the six types:
In other words, spray package failure occurs when the package or product no longer performs to specification.
Incidentally, aerosol spray packages don’t fail by exploding, as components, such as can bodies, bottoms, tops and aerosol valves, are typically crimped together. Components could separate from one another under very high pressures caused by heating the package. However, normal aerosol container pressures are well below the pressures that cause components to separate.
What, then, is the relationship between corrosion and the six forms of spray package failures?
1. A package leaks liquid product or propellant
Pitting corrosion eventually generates a small pin hole that causes leaking in the liquid product area or the gas head space in aerosol containers. A pin hole in the liquid product area of a container allows liquid product to leak, while a pin hole in the vapor area (gas head space) of a container allows propellant (gas) to escape.
However, sometimes product or propellant doesn’t leak from a pin hole when the hole is plugged with metal oxide/hydroxide corrosion product (i.e., a corrosion plug). In other words, gas or liquid leakage occurs either when the pin hole is free from blockage by corrosion products or when a corrosion-plug is porous enough to allow liquid and gas to flow through the pin hole. I have seen numerous instances where perforations (pin holes) were plugged by corrosion product and the container continued to spray.
2. Valves leak propellant
Corrosion pin holes in aerosol valves can also cause the propellant to leak from an aerosol spray package. A pin hole in an aerosol valve must also either be free of corrosion products or have corrosion plugs that are porous enough to allow gas (propellant) to flow through the pin hole.
3. Partially full packages no longer spray
Coating corrosion/delamination and laminate film corrosion/delamination could cause pieces of coating or laminate film to detach from the spray package metal. Free-floating pieces of coating or laminate film could plug valve dip tubes or the valve orifices and cause the packages to stop spraying.
Metal corrosion under a coating, such as detinning, could also cause a coating to become detached from the package metal and subsequently cause the package to stop spraying by plugging valve orifices and dip tubes.
4. Discolored product
The color of steel corrosion product could be black, brown, orange, red or a mixture of several colors. The product could become discolored by the corrosion products when enough metal oxides/hydroxides are either suspended, or dissolved, in the formula.
Aluminum corrosion product could be black, but is typically white. Consequently, discoloration of products by aluminum corrosion products is often harder to see than the corresponding discoloration from steel corrosion products.
5. Product malodor
In some instances, a small amount of metal ions from corrosion does not precipitate from solution and thus remain dissolved in a formula in small concentrations. Dissolved metal ions from corrosion could cause the product to have a malodor.
6. Active ingredients degrade, thereby reducing product efficacy
This final form of package failure is mentioned for the sake of completeness. In some instances, metal ions from corrosion could also cause one or more active ingredients to degrade, resulting in a loss of product efficacy.
Corrosion testing can be used to determine if spray packages will leak; if coating or laminate film might cause packages to stop spraying; and to monitor or predict product discoloration, malodor or active ingredient degradation by metal ions produced by corrosion.
Thanks for your interest and I’ll see you in October. Contact me at 608-831-2076; rustdr@pairodocspro.com or from our two websites: pairodocspro.com and aristartec.com. SPRAY